General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 - 8.88 g/cm³ Show Material materials with Densidad of 8.8 - 8.88 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Dureza Brinell | 20.0 °C | 90 - 180 [-] Show Material materials with Dureza Brinell of 90 - 180 [-] |
Dureza Vickers | 20.0 °C | 95 - 220 [-] Show Material materials with Dureza Vickers of 95 - 220 [-] |
Elongación | 20.0 °C | 6 - 15 % Show Material materials with Elongación of 6 - 15 % |
Elongación A50 | 20.0 °C | 5 - 8 % Show Material materials with Elongación A50 of 5 - 8 % |
Elongation A10 | 20.0 °C | 5 - 8 % Show Material materials with Elongation A10 of 5 - 8 % |
Elongation A100 | 20.0 °C | 4 - 6 % Show Material materials with Elongation A100 of 4 - 6 % |
Límite elástico Rp 0,2 | 20.0 °C | 230 - 620 MPa Show Material materials with Límite elástico Rp 0,2 of 230 - 620 MPa |
Módulo elástico | 20.0 °C | 130 - 143 GPa Show Material materials with Módulo elástico of 130 - 143 GPa |
Resistencia a la tracción | 20.0 °C | 320 - 640 MPa Show Material materials with Resistencia a la tracción of 320 - 640 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) |
Coeficiente de dilatación térmica | 300.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 20.0 °C | 67 - 200 W/(m·K) Show Material materials with Conductividad térmica of 67 - 200 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.00E+7 - 2.60E+7 S/m Show Material materials with Conductividad eléctrica of 1.00E+7 - 2.60E+7 S/m |
Specific Electrical conductivity | 29 - 45 % IACS Show Material materials with Specific Electrical conductivity of 29 - 45 % IACS |
Chemical properties
Property | Value |
---|---|
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 1.6 - 2.5 % Show Material materials with Níquel of 1.6 - 2.5 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % |