Grades provided by the supplier

Grade Shape Equivalent Materials Standard / Norm 

DIN EN CuSn10-C-GS

Casting

DIN EN CuSn10-C-GS, EN CC480K, DIN G-CuSn10, EN 2.1050

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn12-C-GS

Casting

DIN EN CuSn12-C-GS, EN CC483K, DIN G-CuSn12, EN 2.1052

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn12Ni2-C-GS

Casting

DIN EN CuSn12Ni2-C-GS, EN CC484K, DIN G-CuSn12Ni, EN 2.1060

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn53Zn8Pb5-C-GS

Casting

DIN EN CuSn53Zn8Pb5-C-GS, EN CC490K, DIN G-CuSn2ZnPb, EN 2.1098

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn5Zn5Pb5-C-GS

Casting

DIN EN CuSn5Zn5Pb5-C-GS, EN CC491K, DIN G-CuSn5ZnPb, EN 2.1096

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn7Zn2Pb3-C-GS

Casting

DIN EN CuSn7Zn2Pb3-C-GS, EN CC492K, DIN G-CuSn6ZnNi, EN 2.1093

DIN EN 1982, DIN 1705, DIN 1716

DIN EN CuSn7Zn4Pb7-C-GS

Casting

DIN EN CuSn7Zn4Pb7-C-GS, EN CC493K, DIN G-CuSn7ZnPb, EN 2.1090

DIN EN 1982, DIN 1705, DIN 1716

EN CC499K

Casting

EN CC499K, EN CuSn5Zn5Pb2

DIN 50930-6, DIN EN 1982, DIN 1988

EN Cu-ETP

Coil

EN Cu-ETP, EN CW004A, UNS C11000

EN Cu-PHC

Coil

EN Cu-PHC, EN CW020A, UNS C10300

Showing 1 to 10 of 25 entries

Previous

1
2
3

Next

Locations

Germany

Germany

Harkortstraße 5

57462 Olpe,North Rhine-Westphalia

(+49)27618910

United Kingdom

United Kingdom

2 Ripple Court Brockeridge Business Park

GL20 6FG Tewkesbury

(+44)1684854932