General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Dureza Brinell | 20.0 °C | 50 - 120 [-] Show Material materials with Dureza Brinell of 50 - 120 [-] | |
Dureza Vickers | 20.0 °C | 50 [-] Show Material materials with Dureza Vickers of 50 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 80 MPa Show Material materials with Límite elástico Rp 0,2 of 80 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 20.0 °C | 135 GPa Show Material materials with Módulo elástico of 135 GPa | |
Resistencia a la tracción | 20.0 °C | 200 MPa Show Material materials with Resistencia a la tracción of 200 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 300.0 °C | 1.7E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.8E-5 1/K | |
Conductividad térmica | 20.0 °C | 167 - 330 W/(m·K) Show Material materials with Conductividad térmica of 167 - 330 W/(m·K) | |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.60E+7 - 5.40E+7 S/m Show Material materials with Conductividad eléctrica of 2.60E+7 - 5.40E+7 S/m |
Chemical properties
Property | Value |
---|---|
Circonio | 0.1 - 0.2 % Show Material materials with Circonio of 0.1 - 0.2 % |