General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Dureza Brinell | 20.0 °C | 40 - 60 [-] Show Material materials with Dureza Brinell of 40 - 60 [-] | |
Dureza Vickers | 20.0 °C | 40 - 80 [-] Show Material materials with Dureza Vickers of 40 - 80 [-] | |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % | |
Elongation A10 | 20.0 °C | 25 % Show Material materials with Elongation A10 of 25 % | |
Elongation A100 | 20.0 °C | 20 % Show Material materials with Elongation A100 of 20 % | |
Límite elástico Rp 0,2 | 20.0 °C | 40 - 80 MPa Show Material materials with Límite elástico Rp 0,2 of 40 - 80 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 95 - 98 GPa Show Material materials with Módulo elástico of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Resistencia a la tracción | 20.0 °C | 180 - 300 MPa Show Material materials with Resistencia a la tracción of 180 - 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Circonio | 0.1 - 0.2 % Show Material materials with Circonio of 0.1 - 0.2 % |