General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Densidad of 8.8 - 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 160 - 210 [-] Show Material materials with Dureza Brinell of 160 - 210 [-] | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 1.68E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.68E-5 1/K | |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.20E+7 S/m Show Material materials with Conductividad eléctrica of 2.20E+7 S/m |
Specific Electrical conductivity | 38 % IACS Show Material materials with Specific Electrical conductivity of 38 % IACS |
Chemical properties
Property | Value |
---|---|
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 1 - 1.6 % Show Material materials with Níquel of 1 - 1.6 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Silicona | 0.4 - 0.7 % Show Material materials with Silicona of 0.4 - 0.7 % |