General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % | |
Elongation A10 | 20.0 °C | 17 % Show Material materials with Elongation A10 of 17 % | |
Elongation A100 | 20.0 °C | 15 % Show Material materials with Elongation A100 of 15 % | |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 20.0 °C | 410 - 510 MPa Show Material materials with Resistencia a la tracción of 410 - 510 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 0.8 % Show Material materials with Hierro of 0.8 % |
Manganeso | 0.7 % Show Material materials with Manganeso of 0.7 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 0.8 - 2 % Show Material materials with Silicona of 0.8 - 2 % |
Zinc | 1.5 % Show Material materials with Zinc of 1.5 % |