General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.73 - 8.8 g/cm³ Show Material materials with Densidad of 8.73 - 8.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] |
Dureza Vickers | 20.0 °C | 135 - 175 [-] Show Material materials with Dureza Vickers of 135 - 175 [-] |
Módulo de cizallamiento | 20.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa |
Módulo elástico | 20.0 °C | 122 GPa Show Material materials with Módulo elástico of 122 GPa |
100.0 °C | 119 GPa Show Material materials with Módulo elástico of 119 GPa | |
200.0 °C | 114 GPa Show Material materials with Módulo elástico of 114 GPa | |
300.0 °C | 109 GPa Show Material materials with Módulo elástico of 109 GPa | |
400.0 °C | 103 GPa Show Material materials with Módulo elástico of 103 GPa | |
500.0 °C | 94 GPa Show Material materials with Módulo elástico of 94 GPa | |
600.0 °C | 84 GPa Show Material materials with Módulo elástico of 84 GPa | |
700.0 °C | 74 GPa Show Material materials with Módulo elástico of 74 GPa | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 377 - 380 J/(kg·K) Show Material materials with Calor específico of 377 - 380 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Conductividad térmica | 20.0 °C | 159 W/(m·K) Show Material materials with Conductividad térmica of 159 W/(m·K) | |
80.0 °C | 167 W/(m·K) Show Material materials with Conductividad térmica of 167 W/(m·K) | ||
120.0 °C | 172 W/(m·K) Show Material materials with Conductividad térmica of 172 W/(m·K) | ||
160.0 °C | 176 W/(m·K) Show Material materials with Conductividad térmica of 176 W/(m·K) | ||
200.0 °C | 184 W/(m·K) Show Material materials with Conductividad térmica of 184 W/(m·K) | ||
Temperatura de fusión | 875 - 1075 °C Show Material materials with Temperatura de fusión of 875 - 1075 °C | Typical for Wrought Copper Brass |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.10E+7 - 2.11E+7 S/m Show Material materials with Conductividad eléctrica of 2.10E+7 - 2.11E+7 S/m |
Resistividad eléctrica | 20.0 °C | 4.7E-8 Ω·m Show Material materials with Resistividad eléctrica of 4.7E-8 Ω·m |
Specific Electrical conductivity | 36 % IACS Show Material materials with Specific Electrical conductivity of 36 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobre | 84 - 86 % Show Material materials with Cobre of 84 - 86 % |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |