EN 12167 Grade CuNi2Si H150

View suppliers (8)
Want to keep this datasheet? Save it now in your required format

Description

CuNi2Si, mat. No CW111C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBNi2Si, mat. No 2.0855, acc. to DIN 17666 : 1983-12 applies: The material shows favorable electrical and thermal conductivity, corrosion resistance, high fatigue and creep resistance as well as favorable spring properties. CuNi2Si is in hardened condition resistant to stress corrosion. Temperature for removal of workhardening approximates 450°C. Strength still increases at low-temperature range. Processing properties: hot and cold forming: good machinability: moderately soft soldering: good hard soldering: moderately gas shielded welding: moderately burnishing: good Application: Particularly for aerial line material, such as clamps, mounting links, nuts, high-strength and corrosion resistant screws. Furthermore for wire ropes in electrical overhead line construction, bearing bushings, roller bearing cages, valve guide bushings and springs. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.8 - 8.88 g/cm³

Show Material materials with Densidad of 8.8 - 8.88 g/cm³

Mecánica

PropertyTemperatureValue

Coeficiente de Poisson

20.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Dureza Brinell

20.0 °C

150 - 190 [-]

Show Material materials with Dureza Brinell of 150 - 190 [-]

Módulo elástico

20.0 °C

130 - 143 GPa

Show Material materials with Módulo elástico of 130 - 143 GPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

20.0 °C

377 J/(kg·K)

Show Material materials with Calor específico of 377 J/(kg·K)

Coeficiente de dilatación térmica

300.0 °C

1.6E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K

Conductividad térmica

20.0 °C

67 - 200 W/(m·K)

Show Material materials with Conductividad térmica of 67 - 200 W/(m·K)

Eléctrico

PropertyTemperatureValue

Conductividad eléctrica

20.0 °C

1.00E+7 - 2.60E+7 S/m

Show Material materials with Conductividad eléctrica of 1.00E+7 - 2.60E+7 S/m

Specific Electrical conductivity

34 - 45 % IACS

Show Material materials with Specific Electrical conductivity of 34 - 45 % IACS

Chemical properties

PropertyValue

Hierro

0.2 %

Show Material materials with Hierro of 0.2 %

Manganeso

0.1 %

Show Material materials with Manganeso of 0.1 %

Níquel

1.6 - 2.5 %

Show Material materials with Níquel of 1.6 - 2.5 %

Plomo

0.02 %

Show Material materials with Plomo of 0.02 %

Silicona

0.4 - 0.8 %

Show Material materials with Silicona of 0.4 - 0.8 %