General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Densidad | 2.78 g/cm³ Show Material materials with Densidad of 2.78 g/cm³ | T3511 | AA Standards, ASTM B241 | |
2.79 g/cm³ Show Material materials with Densidad of 2.79 g/cm³ | T3511 | Bar, Tube | ||
3.0 g/cm³ Show Material materials with Densidad of 3.0 g/cm³ | T3511 |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Elongación | 7.0 % Show Material materials with Elongación of 7.0 % | T3511 | AA Standards, ASTM B241 | A100 | |
8.8 % Show Material materials with Elongación of 8.8 % | T3511 | ||||
9.0 % Show Material materials with Elongación of 9.0 % | T3511 | AA Standards, ASTM B241 | A100 | ||
10.0 % Show Material materials with Elongación of 10.0 % | T3511 | AA Standards, ASTM B241 | A50 | ||
10.0 - 12.0 % Show Material materials with Elongación of 10.0 - 12.0 % | T3511 | Bar, Tube | |||
Límite elástico | 290.0 MPa Show Material materials with Límite elástico of 290.0 MPa | T3511 | AA Standards, ASTM B241 | RP02 | |
290.0 - 358.0 MPa Show Material materials with Límite elástico of 290.0 - 358.0 MPa | T3511 | Bar, Tube | RP02 | ||
305.0 MPa Show Material materials with Límite elástico of 305.0 MPa | T3511 | AA Standards, ASTM B241 | RP02 | ||
315.0 MPa Show Material materials with Límite elástico of 315.0 MPa | T3511 | AA Standards, ASTM B241 | RP02 | ||
330.0 MPa Show Material materials with Límite elástico of 330.0 MPa | T3511 | AA Standards, ASTM B241 | RP02 | ||
330.0 MPa Show Material materials with Límite elástico of 330.0 MPa | T3511 | ||||
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |||
Módulo elástico | 73.0 GPa Show Material materials with Módulo elástico of 73.0 GPa | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Resistencia a la tracción | 392.0 - 482.0 MPa Show Material materials with Resistencia a la tracción of 392.0 - 482.0 MPa | T3511 | Bar, Tube | ||
395.0 MPa Show Material materials with Resistencia a la tracción of 395.0 MPa | T3511 | AA Standards, ASTM B241 | |||
415.0 MPa Show Material materials with Resistencia a la tracción of 415.0 MPa | T3511 | AA Standards, ASTM B241 | |||
450.0 MPa Show Material materials with Resistencia a la tracción of 450.0 MPa | T3511 | AA Standards, ASTM B241 | |||
470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T3511 | AA Standards, ASTM B241 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Shape | Related Standards |
---|---|---|---|---|---|
Calor específico | 870.0 J/(kg·K) Show Material materials with Calor específico of 870.0 J/(kg·K) | T3511 | |||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T3511 | |||
2.31e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.31e-05 1/K | T3511 | Bar, Tube | |||
20 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | T3511 | AA Standards, ASTM B241 | ||
100 °C | 2.3199999999999998e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3199999999999998e-05 1/K | T3511 | AA Standards, ASTM B241 | ||
Conductividad térmica | 120.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 W/(m·K) | T3511 | |||
121.0 - 193.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 193.0 W/(m·K) | T3511 | AA Standards, ASTM B241 | |||
121.0 - 150.0 W/(m·K) Show Material materials with Conductividad térmica of 121.0 - 150.0 W/(m·K) | T3511 | Bar, Tube | |||
Temperatura de fusión | 500.0 °C Show Material materials with Temperatura de fusión of 500.0 °C | T3511 | |||
505.0 - 635.0 °C Show Material materials with Temperatura de fusión of 505.0 - 635.0 °C | T3511 | AA Standards, ASTM B241 | |||
640.0 °C Show Material materials with Temperatura de fusión of 640.0 °C | T3511 | Bar, Tube |
Eléctrico
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Conductividad eléctrica | 17000000.0 - 29000000.0 S/m Show Material materials with Conductividad eléctrica of 17000000.0 - 29000000.0 S/m | T3511 | AA Standards, ASTM B241 | |
Resistividad eléctrica | 3.45e-08 - 5.88e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.45e-08 - 5.88e-08 Ω·m | T3511 | AA Standards, ASTM B241 | |
4.31e-08 - 5.75e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.31e-08 - 5.75e-08 Ω·m | T3511 | Bar, Tube |
Chemical properties
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Aluminio | 90.7 - 94.7 % Show Material materials with Aluminio of 90.7 - 94.7 % | T3511 | |||
Circonio | 0.2 % Show Material materials with Circonio of 0.2 % | T3511 | |||
Cobre | 3.8 - 4.9 % Show Material materials with Cobre of 3.8 - 4.9 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Hierro | 0.50 % Show Material materials with Hierro of 0.50 % | T3511 | AA Standards, ASTM B241 | ||
0.5 % Show Material materials with Hierro of 0.5 % | T3511 | Bar, Tube | |||
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Manganeso | 0.3 - 0.9 % Show Material materials with Manganeso of 0.3 - 0.9 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T3511 | Bar, Tube | Total | |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T3511 | AA Standards, ASTM B241 | Bar, Tube | |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T3511 | AA Standards, ASTM B241 | Bar, Tube |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, High strength applications | |
Brazing | general: no brazing is known or developed | |
Corrosion properties | Stress corrosion cracking: Betriebsschäden in Gebieten mit Zugspannungen quer zur Kornstruktur, Eingeschränkte Schäden an Laborproben (T4,T3, T351, T3510, T3511), d (T6, T861, T81, T851, T8510, T8511), general: sufficient, in principle it should be protected | |
General machinability | General: poor (O), good to acceptable | |
Workability | general (condition): poor(T4, T3, T351, T3510, T3511, T6), not suitable (T361, T861, T81, T851, T8510, T8511) |