General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 23.0 °C | 17 % Show Material materials with Elongación of 17 % | |
Límite elástico | 23.0 °C | 670 MPa Show Material materials with Límite elástico of 670 MPa | |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
Resistencia a la tracción | 23.0 °C | 1030 MPa Show Material materials with Resistencia a la tracción of 1030 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K |
Conductividad térmica | 23.0 °C | 14 W/(m·K) Show Material materials with Conductividad térmica of 14 W/(m·K) |
Temperatura de fusión | 1370 °C Show Material materials with Temperatura de fusión of 1370 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 0.35 % Show Material materials with Aluminio of 0 - 0.35 % |
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Boro | 0.001 - 0.01 % Show Material materials with Boro of 0.001 - 0.01 % |
Carbono | 0 - 0.08 % Show Material materials with Carbono of 0 - 0.08 % |
Cromo | 13.5 - 16 % Show Material materials with Cromo of 13.5 - 16 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 49.1 - 59.5 % Show Material materials with Hierro of 49.1 - 59.5 % |
Manganeso | 0 - 2 % Show Material materials with Manganeso of 0 - 2 % |
Molibdeno | 1 - 1.5 % Show Material materials with Molibdeno of 1 - 1.5 % |
Níquel | 24 - 27 % Show Material materials with Níquel of 24 - 27 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |
Titanio | 1.9 - 2.4 % Show Material materials with Titanio of 1.9 - 2.4 % |
Vanadio | 0.1 - 0.5 % Show Material materials with Vanadio of 0.1 - 0.5 % |