General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 23.0 °C | 5.8 % Show Material materials with Elongación of 5.8 % | |
Límite elástico | 23.0 °C | 1150 MPa Show Material materials with Límite elástico of 1150 MPa | |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
Resistencia a la tracción | 23.0 °C | 1080 MPa Show Material materials with Resistencia a la tracción of 1080 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K |
Conductividad térmica | 23.0 °C | 16 W/(m·K) Show Material materials with Conductividad térmica of 16 W/(m·K) |
Temperatura de fusión | 1400 °C Show Material materials with Temperatura de fusión of 1400 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Carbono | 0 - 0.07 % Show Material materials with Carbono of 0 - 0.07 % |
Cobre | 3 - 5 % Show Material materials with Cobre of 3 - 5 % |
Cromo | 15 - 17 % Show Material materials with Cromo of 15 - 17 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 69.6 - 79 % Show Material materials with Hierro of 69.6 - 79 % |
Manganeso | 0 - 1.5 % Show Material materials with Manganeso of 0 - 1.5 % |
Molibdeno | 0 - 0.6 % Show Material materials with Molibdeno of 0 - 0.6 % |
Niobio | 0 - 0.45 % Show Material materials with Niobio of 0 - 0.45 % |
Níquel | 3 - 5 % Show Material materials with Níquel of 3 - 5 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |