General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9.9 g/cm³ Show Material materials with Densidad of 9.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 48 % Show Material materials with Elongación of 48 % |
Límite elástico | 23.0 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa |
Resistencia a la tracción | 23.0 °C | 840 MPa Show Material materials with Resistencia a la tracción of 840 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 400 J/(kg·K) Show Material materials with Calor específico of 400 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 23.0 °C | 9 W/(m·K) Show Material materials with Conductividad térmica of 9 W/(m·K) |
Temperatura de fusión | 1300 °C Show Material materials with Temperatura de fusión of 1300 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 - 0.5 % Show Material materials with Aluminio of 0.2 - 0.5 % |
Azufre | 0 - 0.015 % Show Material materials with Azufre of 0 - 0.015 % |
Boro | 0 - 0.015 % Show Material materials with Boro of 0 - 0.015 % |
Carbono | 0.05 - 0.15 % Show Material materials with Carbono of 0.05 - 0.15 % |
Cobalto | 0 - 5 % Show Material materials with Cobalto of 0 - 5 % |
Cromo | 20 - 24 % Show Material materials with Cromo of 20 - 24 % |
Fósforo | 0 - 0.03 % Show Material materials with Fósforo of 0 - 0.03 % |
Hierro | 0 - 3 % Show Material materials with Hierro of 0 - 3 % |
Lantano | 0.01 - 0.05 % Show Material materials with Lantano of 0.01 - 0.05 % |
Manganeso | 0.3 - 1 % Show Material materials with Manganeso of 0.3 - 1 % |
Molibdeno | 1 - 3 % Show Material materials with Molibdeno of 1 - 3 % |
Níquel | 47.5 - 65.2 % Show Material materials with Níquel of 47.5 - 65.2 % |
Silicona | 0.25 - 0.75 % Show Material materials with Silicona of 0.25 - 0.75 % |
Wolframio | 13 - 15 % Show Material materials with Wolframio of 13 - 15 % |