Acero bajo en carbono
EN 10025-3 Grade S420N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10025-3 Grade S420NL normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
7000 Serie
AA Standards Grade 7075 T7351Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-3 Grade S460N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-3 Grade S460NL normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML1 thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch