General
Property | Value | Condition |
---|---|---|
Densidad | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ | T8 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |
Elongación | 9.0 % Show Material materials with Elongación of 9.0 % | T8 | |
Límite elástico | 340.0 MPa Show Material materials with Límite elástico of 340.0 MPa | T8 | |
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |
Módulo elástico | 74.0 GPa Show Material materials with Módulo elástico of 74.0 GPa | T8 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |
Resistencia a la tracción | 450.0 MPa Show Material materials with Resistencia a la tracción of 450.0 MPa | T8 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 860.0 J/(kg·K) Show Material materials with Calor específico of 860.0 J/(kg·K) | T8 |
Coeficiente de dilatación térmica | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T8 |
Conductividad térmica | 130.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 W/(m·K) | T8 |
Temperatura de fusión | 540.0 °C Show Material materials with Temperatura de fusión of 540.0 °C | T8 |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 91.5 - 93.8 % Show Material materials with Aluminio of 91.5 - 93.8 % | T8 |
Circonio | 0.1 - 0.25 % Show Material materials with Circonio of 0.1 - 0.25 % | T8 |
Cobre | 5.8 - 6.8 % Show Material materials with Cobre of 5.8 - 6.8 % | T8 |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % | T8 |
Magnesio | 0.02 % Show Material materials with Magnesio of 0.02 % | T8 |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % | T8 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T8 |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | T8 |
Titanio | 0.02 - 0.1 % Show Material materials with Titanio of 0.02 - 0.1 % | T8 |
Vanadio | 0.05 - 0.15 % Show Material materials with Vanadio of 0.05 - 0.15 % | T8 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T8 |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |