General
Property | Value | Condition |
---|---|---|
Densidad | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ | T61 |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | T61 | |||
Dureza Brinell | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
110 [-] Show Material materials with Dureza Brinell of 110 [-] | T61 | 500 kg load, 10 mm b | |||
110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T61 | Pink Sheets, ASTM B108 | Casting | ||
Elongación | 0.5 % Show Material materials with Elongación of 0.5 % | T61 | |||
0.5 % Show Material materials with Elongación of 0.5 % | T61 | Sand cast, elongation in 50 mm | |||
Límite elástico | 140.0 MPa Show Material materials with Límite elástico of 140.0 MPa | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | RP02 |
220.0 MPa Show Material materials with Límite elástico of 220.0 MPa | T61 | ||||
290 MPa Show Material materials with Límite elástico of 290 MPa | T61 | Sand cast, RP02 | |||
Módulo de cizallamiento | 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.5 GPa | T61 | |||
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T61 | |||
71 GPa Show Material materials with Módulo elástico of 71 GPa | T61 | ||||
Resistencia a la fatiga | 65 MPa Show Material materials with Resistencia a la fatiga of 65 MPa | T61 | for 5x10⁸ cycles, R.R. Moore type test | ||
Resistencia a la tracción | 220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | T61 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | T61 | ||||
275.0 MPa Show Material materials with Resistencia a la tracción of 275.0 MPa | T61 | Pink Sheets, ASTM B108 | Casting | ||
324 MPa Show Material materials with Resistencia a la tracción of 324 MPa | T61 | Sand cast | |||
Resistencia al cizallamiento | 240 MPa Show Material materials with Resistencia al cizallamiento of 240 MPa | T61 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 960.0 J/(kg·K) Show Material materials with Calor específico of 960.0 J/(kg·K) | T61 | ||||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T61 | ||||
100 °C | 0.0000225 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000225 1/K | T61 | nominal value between 20°C and the mentioned temperature | |||
300 °C | 0.0000245 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000245 1/K | T61 | nominal value between 20°C and the mentioned temperature | |||
Conductividad térmica | 130.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 W/(m·K) | T61 | ||||
25 °C | 134 W/(m·K) Show Material materials with Conductividad térmica of 134 W/(m·K) | T61 | nominal value | |||
Temperatura de fusión | 532.0 - 635.0 °C Show Material materials with Temperatura de fusión of 532.0 - 635.0 °C | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | ||
540.0 °C Show Material materials with Temperatura de fusión of 540.0 °C | T61 |
Eléctrico
Property | Value | Condition | Comment |
---|---|---|---|
Conductividad eléctrica | 19500000 S/m Show Material materials with Conductividad eléctrica of 19500000 S/m | T61 | Typical/Derived values |
Resistividad eléctrica | 5.2200000000000004e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.2200000000000004e-08 Ω·m | T61 | Typical values |
Specific Electrical conductivity | 33.0 - 34.0 % IACS Show Material materials with Specific Electrical conductivity of 33.0 - 34.0 % IACS | T61 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 88.4 - 93.6 % Show Material materials with Aluminio of 88.4 - 93.6 % | T61 | ||
Cobre | 3.5 - 4.5 % Show Material materials with Cobre of 3.5 - 4.5 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Hierro | 1.0 % Show Material materials with Hierro of 1.0 % | T61 | ||
1.00 % Show Material materials with Hierro of 1.00 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting | |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Níquel | 1.7 - 2.3 % Show Material materials with Níquel of 1.7 - 2.3 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T61 | ||
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T61 | Pink Sheets, ASTM B108, ASTM B26, ASTM B618 | Casting |