General
Property | Value | Condition |
---|---|---|
Densidad | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ | T7 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |
Elongación | 1.5 % Show Material materials with Elongación of 1.5 % | T7 | |
Límite elástico | 200.0 MPa Show Material materials with Límite elástico of 200.0 MPa | T7 | |
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T7 | |
Resistencia a la tracción | 240.0 MPa Show Material materials with Resistencia a la tracción of 240.0 MPa | T7 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 960.0 J/(kg·K) Show Material materials with Calor específico of 960.0 J/(kg·K) | T7 |
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T7 |
Conductividad térmica | 150.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 W/(m·K) | T7 |
Temperatura de fusión | 540.0 °C Show Material materials with Temperatura de fusión of 540.0 °C | T7 |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 16000000.0 - 23000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 88.4 - 93.6 % Show Material materials with Aluminio of 88.4 - 93.6 % | T7 |
Cobre | 3.5 - 4.5 % Show Material materials with Cobre of 3.5 - 4.5 % | T7 |
Cromo | 0.25 % Show Material materials with Cromo of 0.25 % | T7 |
Hierro | 1.0 % Show Material materials with Hierro of 1.0 % | T7 |
Magnesio | 1.2 - 1.8 % Show Material materials with Magnesio of 1.2 - 1.8 % | T7 |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T7 |
Níquel | 1.7 - 2.3 % Show Material materials with Níquel of 1.7 - 2.3 % | T7 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T7 |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % | T7 |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T7 |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T7 |