General
Property | Value | Condition |
---|---|---|
Densidad | 3.0 g/cm³ Show Material materials with Densidad of 3.0 g/cm³ | T5 |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | T5 | |||
Compressive yield strength | 138 MPa Show Material materials with Compressive yield strength of 138 MPa | T5 | |||
Dureza Brinell | 80 [-] Show Material materials with Dureza Brinell of 80 [-] | T5 | 500 kg load, 10 mm b | ||
80.0 [-] Show Material materials with Dureza Brinell of 80.0 [-] | T5 | Pink Sheets, ASTM B26 | Casting | ||
Elongación | 1.5 % Show Material materials with Elongación of 1.5 % | T5 | Sand cast, elongation in 50 mm | ||
1.8 % Show Material materials with Elongación of 1.8 % | T5 | ||||
Límite elástico | 179 MPa Show Material materials with Límite elástico of 179 MPa | T5 | Sand cast, RP02 | ||
180.0 MPa Show Material materials with Límite elástico of 180.0 MPa | T5 | ||||
Módulo de cizallamiento | 28.0 GPa Show Material materials with Módulo de cizallamiento of 28.0 GPa | T5 | |||
Módulo elástico | 74 GPa Show Material materials with Módulo elástico of 74 GPa | T5 | |||
78.0 GPa Show Material materials with Módulo elástico of 78.0 GPa | T5 | ||||
Resistencia a la fatiga | 76 MPa Show Material materials with Resistencia a la fatiga of 76 MPa | T5 | for 5x10⁸ cycles, R.R. Moore type test | ||
Resistencia a la tracción | 170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | T5 | Pink Sheets, ASTM B26 | Casting | |
200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | T5 | ||||
207 MPa Show Material materials with Resistencia a la tracción of 207 MPa | T5 | Sand cast | |||
Resistencia al cizallamiento | 165 MPa Show Material materials with Resistencia al cizallamiento of 165 MPa | T5 |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Calor específico | 860.0 J/(kg·K) Show Material materials with Calor específico of 860.0 J/(kg·K) | T5 | ||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T5 | ||
Conductividad térmica | 110.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 W/(m·K) | T5 | ||
Temperatura de fusión | 510.0 - 607.0 °C Show Material materials with Temperatura de fusión of 510.0 - 607.0 °C | T5 | Pink Sheets, ASTM B26 | Casting |
540.0 °C Show Material materials with Temperatura de fusión of 540.0 °C | T5 |
Eléctrico
Property | Value | Condition | Comment |
---|---|---|---|
Resistividad eléctrica | 6.39e-08 Ω·m Show Material materials with Resistividad eléctrica of 6.39e-08 Ω·m | T5 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 85.8 - 91.5 % Show Material materials with Aluminio of 85.8 - 91.5 % | T5 | ||
Cobre | 3.0 - 4.0 % Show Material materials with Cobre of 3.0 - 4.0 % | T5 | Pink Sheets, ASTM B26 | Casting |
Hierro | 1.0 % Show Material materials with Hierro of 1.0 % | T5 | ||
1.00 % Show Material materials with Hierro of 1.00 % | T5 | Pink Sheets, ASTM B26 | Casting | |
Magnesio | 0.1 % Show Material materials with Magnesio of 0.1 % | T5 | Pink Sheets, ASTM B26 | Casting |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % | T5 | Pink Sheets, ASTM B26 | Casting |
Níquel | 0.35 % Show Material materials with Níquel of 0.35 % | T5 | Pink Sheets, ASTM B26 | Casting |
Otro | 0.5 % Show Material materials with Otro of 0.5 % | T5 | ||
Silicona | 5.5 - 6.5 % Show Material materials with Silicona of 5.5 - 6.5 % | T5 | Pink Sheets, ASTM B26 | Casting |
Titanio | 0.25 % Show Material materials with Titanio of 0.25 % | T5 | Pink Sheets, ASTM B26 | Casting |
Zinc | 1.0 % Show Material materials with Zinc of 1.0 % | T5 | Pink Sheets, ASTM B26 | Casting |