General
Property | Value | Condition |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | H15 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | |
Elongación | 3.5 % Show Material materials with Elongación of 3.5 % | H15 | |
Límite elástico | 210.0 MPa Show Material materials with Límite elástico of 210.0 MPa | H15 | |
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | |
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | H15 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | |
Resistencia a la tracción | 270.0 MPa Show Material materials with Resistencia a la tracción of 270.0 MPa | H15 |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | H15 | |
Coeficiente de dilatación térmica | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | H15 | |
Conductividad térmica | 140.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 W/(m·K) | H15 | |
Temperatura de fusión | 620.0 °C Show Material materials with Temperatura de fusión of 620.0 °C | H15 | |
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 94.7 - 97.9 % Show Material materials with Aluminio of 94.7 - 97.9 % | H15 |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H15 |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | H15 |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % | H15 |
Magnesio | 1.6 - 2.5 % Show Material materials with Magnesio of 1.6 - 2.5 % | H15 |
Manganeso | 0.5 - 1.1 % Show Material materials with Manganeso of 0.5 - 1.1 % | H15 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | H15 |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | H15 |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | H15 |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % | H15 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |