Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 900 J/(kg·K) Show Material materials with Calor específico of 900 J/(kg·K) |
Coeficiente de dilatación térmica | 20.0 °C | 2.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K |
Conductividad térmica | 20.0 °C | 130 W/(m·K) Show Material materials with Conductividad térmica of 130 W/(m·K) |
Temperatura de fusión | 590 °C Show Material materials with Temperatura de fusión of 590 °C |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 67 [-] Show Material materials with Dureza Brinell of 67 [-] |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % |
Elongación A50 | 20.0 °C | 5 - 15 % Show Material materials with Elongación A50 of 5 - 15 % |
Límite elástico | 20.0 °C | 200 MPa Show Material materials with Límite elástico of 200 MPa |
Límite elástico Rp 0,2 | 20.0 °C | 180 - 205 MPa Show Material materials with Límite elástico Rp 0,2 of 180 - 205 MPa |
Módulo elástico | 20.0 °C | 70 GPa Show Material materials with Módulo elástico of 70 GPa |
Resistencia a la tracción | 20.0 °C | 250 - 270 MPa Show Material materials with Resistencia a la tracción of 250 - 270 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 94.4 - 96.8 % Show Material materials with Aluminio of 94.4 - 96.8 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Cromo | 0.15 - 0.35 % Show Material materials with Cromo of 0.15 - 0.35 % |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % |
Magnesio | 3.1 - 3.9 % Show Material materials with Magnesio of 3.1 - 3.9 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Otro | 0.15 % Show Material materials with Otro of 0.15 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |