General
Property | Value | Condition |
---|---|---|
Densidad | 2.69 g/cm³ Show Material materials with Densidad of 2.69 g/cm³ | H112 |
2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | H112 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||
Dureza Brinell | 62.0 [-] Show Material materials with Dureza Brinell of 62.0 [-] | H112 | AA Standards | |
62.0 [-] Show Material materials with Dureza Brinell of 62.0 [-] | H112 | 500 kg load, 10 mm ball | ||
Elongación | 8.0 % Show Material materials with Elongación of 8.0 % | H112 | AA Standards, ASTM B209, ASTM B547 | A50 |
9.0 % Show Material materials with Elongación of 9.0 % | H112 | AA Standards, ASTM B209 | A100 | |
10.0 % Show Material materials with Elongación of 10.0 % | H112 | AA Standards, ASTM B221, ASTM B241 | A100 | |
12.0 % Show Material materials with Elongación of 12.0 % | H112 | AA Standards, ASTM B221, ASTM B241 | A50 | |
13.0 % Show Material materials with Elongación of 13.0 % | H112 | AA Standards, ASTM B209 | A100 | |
14.0 % Show Material materials with Elongación of 14.0 % | H112 | |||
18.0 % Show Material materials with Elongación of 18.0 % | H112 | AA Standards | A50 | |
18 % Show Material materials with Elongación of 18 % | H112 | |||
Límite elástico | 85.0 MPa Show Material materials with Límite elástico of 85.0 MPa | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241 | RP02 |
110.0 MPa Show Material materials with Límite elástico of 110.0 MPa | H112 | |||
125.0 MPa Show Material materials with Límite elástico of 125.0 MPa | H112 | AA Standards, ASTM B209, ASTM B547 | RP02 | |
125 MPa Show Material materials with Límite elástico of 125 MPa | H112 | RP02 | ||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||
Módulo de compresión | 71.0 MPa Show Material materials with Módulo de compresión of 71.0 MPa | H112 | ||
Módulo elástico | 70 GPa Show Material materials with Módulo elástico of 70 GPa | H112 | ||
71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | H112 | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||
Resistencia a la tracción | 215.0 MPa Show Material materials with Resistencia a la tracción of 215.0 MPa | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241 | |
220.0 MPa Show Material materials with Resistencia a la tracción of 220.0 MPa | H112 | AA Standards, ASTM B209, ASTM B547 | ||
250.0 MPa Show Material materials with Resistencia a la tracción of 250.0 MPa | H112 | AA Standards | ||
250 MPa Show Material materials with Resistencia a la tracción of 250 MPa | H112 | |||
Resistencia al cizallamiento | 159.0 MPa Show Material materials with Resistencia al cizallamiento of 159.0 MPa | H112 |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | H112 | |
Coeficiente de dilatación térmica | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | H112 | |
Conductividad térmica | 130.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 W/(m·K) | H112 | |
Temperatura de fusión | 600.0 °C Show Material materials with Temperatura de fusión of 600.0 °C | H112 | |
Temperatura máx. de funcionamiento | 150.0 °C Show Material materials with Temperatura máx. de funcionamiento of 150.0 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 31000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 31000000.0 S/m | Typical for Wrought 5000 Series Aluminium |
Resistividad eléctrica | 3.3e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.3e-08 - 5e-08 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 94.5 - 97.1 % Show Material materials with Aluminio of 94.5 - 97.1 % | H112 | |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Cromo | 0.05 - 0.2 % Show Material materials with Cromo of 0.05 - 0.2 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Hierro | 0.40 % Show Material materials with Hierro of 0.40 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
0.4 % Show Material materials with Hierro of 0.4 % | H112 | ||
Magnesio | 2.4 - 3.0 % Show Material materials with Magnesio of 2.4 - 3.0 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Manganeso | 0.5 - 1.0 % Show Material materials with Manganeso of 0.5 - 1.0 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | H112 | |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | H112 | AA Standards, ASTM B209, ASTM B221, ASTM B241, ASTM B547 |
Technological properties
Property | ||
---|---|---|
Brazing | general: no brazing is known or developed | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (O, H32, H111), sufficient (H34) | |
Workability | general (condition): good (O), acceptable (H32, H34, H111) |