General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | T1 | AA Standards, ASTM B221 |
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||
Elongación | 14.0 % Show Material materials with Elongación of 14.0 % | T1 | AA Standards, ASTM B221 | A100 |
16.0 % Show Material materials with Elongación of 16.0 % | T1 | AA Standards, ASTM B221 | A50 | |
16.0 % Show Material materials with Elongación of 16.0 % | T1 | |||
Límite elástico | 105.0 MPa Show Material materials with Límite elástico of 105.0 MPa | T1 | AA Standards, ASTM B221 | RP02 |
120.0 MPa Show Material materials with Límite elástico of 120.0 MPa | T1 | |||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | T1 | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||
Resistencia a la tracción | 170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | T1 | AA Standards, ASTM B221 | |
200.0 MPa Show Material materials with Resistencia a la tracción of 200.0 MPa | T1 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | T1 | ||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T1 | ||
20 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | T1 | AA Standards, ASTM B221 | |
100 °C | 2.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.36e-05 1/K | T1 | AA Standards, ASTM B221 | |
Conductividad térmica | 180.0 - 188.0 W/(m·K) Show Material materials with Conductividad térmica of 180.0 - 188.0 W/(m·K) | T1 | AA Standards, ASTM B221 | |
180.0 W/(m·K) Show Material materials with Conductividad térmica of 180.0 W/(m·K) | T1 | |||
Temperatura de fusión | 605.0 - 655.0 °C Show Material materials with Temperatura de fusión of 605.0 - 655.0 °C | T1 | AA Standards, ASTM B221 | |
610.0 °C Show Material materials with Temperatura de fusión of 610.0 °C | T1 |
Eléctrico
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Conductividad eléctrica | 27000000.0 - 28000000.0 S/m Show Material materials with Conductividad eléctrica of 27000000.0 - 28000000.0 S/m | T1 | AA Standards, ASTM B221 | |
27000000 S/m Show Material materials with Conductividad eléctrica of 27000000 S/m | T1 | Typical value | ||
Resistividad eléctrica | 3.57e-08 - 3.7e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.57e-08 - 3.7e-08 Ω·m | T1 | AA Standards, ASTM B221 | |
3.6499999999999996e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.6499999999999996e-08 Ω·m | T1 | Typical value | ||
Specific Electrical conductivity | 47.0 % IACS Show Material materials with Specific Electrical conductivity of 47.0 % IACS | T1 | Typical/Derived value |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 97.5 - 99.0 % Show Material materials with Aluminio of 97.5 - 99.0 % | T1 | |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T1 | AA Standards, ASTM B221 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T1 | AA Standards, ASTM B221 |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | T1 | AA Standards, ASTM B221 |
0.35 % Show Material materials with Hierro of 0.35 % | T1 | ||
Magnesio | 0.4 - 0.6 % Show Material materials with Magnesio of 0.4 - 0.6 % | T1 | AA Standards, ASTM B221 |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T1 | AA Standards, ASTM B221 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T1 | |
Silicona | 0.6 - 0.9 % Show Material materials with Silicona of 0.6 - 0.9 % | T1 | AA Standards, ASTM B221 |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | T1 | AA Standards, ASTM B221 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T1 | AA Standards, ASTM B221 |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Workability | Excellent workability. |