General
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |
Elongación | 17.0 % Show Material materials with Elongación of 17.0 % | T4 | |
Hardness, Rockwell Superficial 15-T | 70.0 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 70.0 [-] | T4 | |
Límite elástico | 100.0 MPa Show Material materials with Límite elástico of 100.0 MPa | T4 | |
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |
Módulo de compresión | 69.6 MPa Show Material materials with Módulo de compresión of 69.6 MPa | T4 | |
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | T4 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |
Resistencia a la fatiga | 97 MPa Show Material materials with Resistencia a la fatiga of 97 MPa | T4 | Min., for 5x10⁸ cycles |
Resistencia a la tracción | 210.0 MPa Show Material materials with Resistencia a la tracción of 210.0 MPa | T4 | |
Resistencia al cizallamiento | 152.0 MPa Show Material materials with Resistencia al cizallamiento of 152.0 MPa | T4 |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | T4 | |
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4 | |
Conductividad térmica | 170.0 - 220.0 W/(m·K) Show Material materials with Conductividad térmica of 170.0 - 220.0 W/(m·K) | Typical for Wrought 6000 Series Aluminium | |
Temperatura de fusión | 610.0 °C Show Material materials with Temperatura de fusión of 610.0 °C | T4 |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 21000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
Resistividad eléctrica | 2.9e-08 - 5e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 97.5 - 99.0 % Show Material materials with Aluminio of 97.5 - 99.0 % | T4 |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T4 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T4 |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | T4 |
Magnesio | 0.4 - 0.6 % Show Material materials with Magnesio of 0.4 - 0.6 % | T4 |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T4 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T4 |
Silicona | 0.6 - 0.9 % Show Material materials with Silicona of 0.6 - 0.9 % | T4 |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | T4 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T4 |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |