General
Mecánica
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | T4 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | A100 |
14.0 % Show Material materials with Elongación of 14.0 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | A50 | |
16.0 % Show Material materials with Elongación of 16.0 % | T4 | AA Standards, ASTM B210, ASTM B483 | A50 | |
16.0 % Show Material materials with Elongación of 16.0 % | T4 | AA Standards, ASTM B210, ASTM B483 | A100 | |
17.0 % Show Material materials with Elongación of 17.0 % | T4 | |||
18.0 % Show Material materials with Elongación of 18.0 % | T4 | AA Standards, ASTM B210, ASTM B483 | A50 | |
22.0 % Show Material materials with Elongación of 22.0 % | T4 | AA Standards | A50 | |
22 % Show Material materials with Elongación of 22 % | T4 | |||
Límite elástico | 60.0 MPa Show Material materials with Límite elástico of 60.0 MPa | T4 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | RP02 |
70.0 MPa Show Material materials with Límite elástico of 70.0 MPa | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | RP02 | |
83.0 MPa Show Material materials with Límite elástico of 83.0 MPa | T4 | |||
90.0 MPa Show Material materials with Límite elástico of 90.0 MPa | T4 | AA Standards | RP02 | |
90 MPa Show Material materials with Límite elástico of 90 MPa | T4 | RP02 | ||
Módulo de cizallamiento | 26.0 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||
Módulo de compresión | 69.7 MPa Show Material materials with Módulo de compresión of 69.7 MPa | T4 | ||
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | |
69 GPa Show Material materials with Módulo elástico of 69 GPa | T4 | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||
Resistencia a la tracción | 125.0 MPa Show Material materials with Resistencia a la tracción of 125.0 MPa | T4 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | |
130.0 MPa Show Material materials with Resistencia a la tracción of 130.0 MPa | T4 | AA Standards, ASTM B221, ASTM B241, ASTM B345 | ||
150.0 MPa Show Material materials with Resistencia a la tracción of 150.0 MPa | T4 | AA Standards, ASTM B210, ASTM B483 | ||
160.0 MPa Show Material materials with Resistencia a la tracción of 160.0 MPa | T4 | |||
170.0 MPa Show Material materials with Resistencia a la tracción of 170.0 MPa | T4 | AA Standards | ||
170 MPa Show Material materials with Resistencia a la tracción of 170 MPa | T4 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | T4 | ||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4 | ||
20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3399999999999996e-05 1/K | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | |
Conductividad térmica | 193.0 - 218.0 W/(m·K) Show Material materials with Conductividad térmica of 193.0 - 218.0 W/(m·K) | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | |
200.0 W/(m·K) Show Material materials with Conductividad térmica of 200.0 W/(m·K) | T4 | |||
Temperatura de fusión | 615.0 - 655.0 °C Show Material materials with Temperatura de fusión of 615.0 - 655.0 °C | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 | |
620.0 °C Show Material materials with Temperatura de fusión of 620.0 °C | T4 |
Eléctrico
Property | Value | Condition | Related Standards |
---|---|---|---|
Conductividad eléctrica | 29000000.0 - 34000000.0 S/m Show Material materials with Conductividad eléctrica of 29000000.0 - 34000000.0 S/m | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Resistividad eléctrica | 2.94e-08 - 3.45e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.94e-08 - 3.45e-08 Ω·m | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 97.5 - 99.4 % Show Material materials with Aluminio of 97.5 - 99.4 % | T4 | |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Hierro | 0.35 % Show Material materials with Hierro of 0.35 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
0.35 % Show Material materials with Hierro of 0.35 % | T4 | ||
Magnesio | 0.45 - 0.9 % Show Material materials with Magnesio of 0.45 - 0.9 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T4 | |
Silicona | 0.2 - 0.6 % Show Material materials with Silicona of 0.2 - 0.6 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T4 | AA Standards, ASTM B210, ASTM B221, ASTM B241, ASTM B345, ASTM B483 |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (T1, T4), sufficient (T5, T452, T6, T83, T831, T832) | |
Workability | general (condition): acceptable (T1, T4, T5, T452), poor(T6, T83, T831, T832) |