General
Property | Value | Condition |
---|---|---|
Densidad | 2.78 g/cm³ Show Material materials with Densidad of 2.78 g/cm³ | T6 |
2.9 g/cm³ Show Material materials with Densidad of 2.9 g/cm³ | T6 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | |
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | T6 | |
Límite elástico | 310.0 MPa Show Material materials with Límite elástico of 310.0 MPa | T6 | |
Módulo de cizallamiento | 26.9 GPa Show Material materials with Módulo de cizallamiento of 26.9 GPa | T6 | |
Módulo de compresión | 72.4 MPa Show Material materials with Módulo de compresión of 72.4 MPa | T6 | |
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T6 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | |
Resistencia a la tracción | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | T6 | |
Resistencia al cizallamiento | 214.0 MPa Show Material materials with Resistencia al cizallamiento of 214.0 MPa | T6 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Comment |
---|---|---|---|---|
Calor específico | 880.0 J/(kg·K) Show Material materials with Calor específico of 880.0 J/(kg·K) | T6 | ||
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T6 | ||
Conductividad térmica | 140.0 W/(m·K) Show Material materials with Conductividad térmica of 140.0 W/(m·K) | T6 | ||
20 °C | 137 W/(m·K) Show Material materials with Conductividad térmica of 137 W/(m·K) | T6 | unstated value | |
Temperatura de fusión | 610.0 °C Show Material materials with Temperatura de fusión of 610.0 °C | T6 |
Eléctrico
Property | Value | Condition | Comment |
---|---|---|---|
Conductividad eléctrica | 20300000 S/m Show Material materials with Conductividad eléctrica of 20300000 S/m | T6 | Typical/derived value |
Resistividad eléctrica | 2.9e-08 - 5.6e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.9e-08 - 5.6e-08 Ω·m | Typical for Wrought 7000 Series Aluminium | |
Specific Electrical conductivity | 35.0 % IACS Show Material materials with Specific Electrical conductivity of 35.0 % IACS | T6 | Typical value |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 91.0 - 94.7 % Show Material materials with Aluminio of 91.0 - 94.7 % | T6 |
Circonio | 0.08 - 0.2 % Show Material materials with Circonio of 0.08 - 0.2 % | T6 |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | T6 |
Cromo | 0.06 - 0.2 % Show Material materials with Cromo of 0.06 - 0.2 % | T6 |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | T6 |
Magnesio | 1.0 - 1.8 % Show Material materials with Magnesio of 1.0 - 1.8 % | T6 |
Manganeso | 0.2 - 0.7 % Show Material materials with Manganeso of 0.2 - 0.7 % | T6 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T6 |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % | T6 |
Titanio | 0.01 - 0.06 % Show Material materials with Titanio of 0.01 - 0.06 % | T6 |
Zinc | 4.0 - 5.0 % Show Material materials with Zinc of 4.0 - 5.0 % | T6 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent |