Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 910 J/(kg·K) Show Material materials with Calor específico of 910 J/(kg·K) |
Coeficiente de dilatación térmica | 20.0 °C | 2.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K |
Conductividad térmica | 20.0 °C | 130 W/(m·K) Show Material materials with Conductividad térmica of 130 W/(m·K) |
Temperatura de fusión | 480 °C Show Material materials with Temperatura de fusión of 480 °C |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 5.5 % Show Material materials with Elongación of 5.5 % |
Elongación A50 | 20.0 °C | 5 - 9 % Show Material materials with Elongación A50 of 5 - 9 % |
Límite elástico | 20.0 °C | 470 MPa Show Material materials with Límite elástico of 470 MPa |
Límite elástico Rp 0,2 | 20.0 °C | 370 - 505 MPa Show Material materials with Límite elástico Rp 0,2 of 370 - 505 MPa |
Módulo elástico | 20.0 °C | 72 GPa Show Material materials with Módulo elástico of 72 GPa |
Resistencia a la tracción | 20.0 °C | 460 - 570 MPa Show Material materials with Resistencia a la tracción of 460 - 570 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 86.9 - 91.4 % Show Material materials with Aluminio of 86.9 - 91.4 % |
Circonio | 0.25 % Show Material materials with Circonio of 0.25 % |
Cobre | 1.2 - 2 % Show Material materials with Cobre of 1.2 - 2 % |
Cromo | 0.18 - 0.28 % Show Material materials with Cromo of 0.18 - 0.28 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Magnesio | 2.1 - 2.9 % Show Material materials with Magnesio of 2.1 - 2.9 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Otro | 0.15 % Show Material materials with Otro of 0.15 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Zinc | 5.1 - 6.1 % Show Material materials with Zinc of 5.1 - 6.1 % |