General
Property | Value | Condition |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | T6 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |
Elongación | 4.0 % Show Material materials with Elongación of 4.0 % | T6 | |
Límite elástico | 170.0 MPa Show Material materials with Límite elástico of 170.0 MPa | T6 | |
Módulo de cizallamiento | 2.8 GPa Show Material materials with Módulo de cizallamiento of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T6 | |
Resistencia a la tracción | 310.0 MPa Show Material materials with Resistencia a la tracción of 310.0 MPa | T6 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 960.0 J/(kg·K) Show Material materials with Calor específico of 960.0 J/(kg·K) | T6 |
Coeficiente de dilatación térmica | 2.2e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2e-05 1/K | T6 |
Conductividad térmica | 110.0 W/(m·K) Show Material materials with Conductividad térmica of 110.0 W/(m·K) | T6 |
Temperatura de fusión | 590.0 °C Show Material materials with Temperatura de fusión of 590.0 °C | T6 |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 85.8 - 90.6 % Show Material materials with Aluminio of 85.8 - 90.6 % | T6 |
Cobre | 0.6 % Show Material materials with Cobre of 0.6 % | T6 |
Estaño | 0.15 % Show Material materials with Estaño of 0.15 % | T6 |
Hierro | 1.3 % Show Material materials with Hierro of 1.3 % | T6 |
Magnesio | 0.4 - 0.6 % Show Material materials with Magnesio of 0.4 - 0.6 % | T6 |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % | T6 |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | T6 |
Otro | 0.25 % Show Material materials with Otro of 0.25 % | T6 |
Silicona | 9.0 - 10.0 % Show Material materials with Silicona of 9.0 - 10.0 % | T6 |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | T6 |