General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación | 23.0 °C | 35 % Show Material materials with Elongación of 35 % | |
Límite elástico | 23.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
Resistencia a la tracción | 23.0 °C | 590 MPa Show Material materials with Resistencia a la tracción of 590 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 480 J/(kg·K) Show Material materials with Calor específico of 480 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K |
Conductividad térmica | 23.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) |
Temperatura de fusión | 1380 °C Show Material materials with Temperatura de fusión of 1380 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Boro | 1.5E-3 - 5E-3 % Show Material materials with Boro of 1.5E-3 - 5E-3 % |
Carbono | 0 - 0.04 % Show Material materials with Carbono of 0 - 0.04 % |
Cromo | 16 - 18.5 % Show Material materials with Cromo of 16 - 18.5 % |
Fósforo | 0 - 0.05 % Show Material materials with Fósforo of 0 - 0.05 % |
Hierro | 61.2 - 71.9 % Show Material materials with Hierro of 61.2 - 71.9 % |
Manganeso | 0 - 2 % Show Material materials with Manganeso of 0 - 2 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Nitrógeno | 0.1 - 0.22 % Show Material materials with Nitrógeno of 0.1 - 0.22 % |
Níquel | 10 - 14 % Show Material materials with Níquel of 10 - 14 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |