General
Property | Value | Condition | Related Standards |
---|---|---|---|
Densidad | 4.42 g/cm³ Show Material materials with Densidad of 4.42 g/cm³ | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Mecánica
Property | Value | Condition | Related Standards |
---|---|---|---|
Módulo elástico | 105.0 - 120.0 GPa Show Material materials with Módulo elástico of 105.0 - 120.0 GPa | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Resistencia a la tracción | 950.0 - 1100.0 MPa Show Material materials with Resistencia a la tracción of 950.0 - 1100.0 MPa | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Aplicaciones térmicas
Property | Value | Condition | Related Standards |
---|---|---|---|
Coeficiente de dilatación térmica | 9e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 9e-06 1/K | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Temperatura de fusión | 1605.0 °C Show Material materials with Temperatura de fusión of 1605.0 °C | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 5.5 - 6.75 % Show Material materials with Aluminio of 5.5 - 6.75 % | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Hierro | 0.4 Show Material materials with Hierro of 0.4 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Oxígeno | 0.2 Show Material materials with Oxígeno of 0.2 | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | Annealed | AMS 4928, ASTM B348, ASTM F136 |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Jewellery, Chemical, Springs, Bolts, Fasteners |