General
Property | Value | Condition |
---|---|---|
Densidad | 2.7 g/cm³ Show Material materials with Densidad of 2.7 g/cm³ | H111 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |
Límite elástico | 29.0 MPa Show Material materials with Límite elástico of 29.0 MPa | H111 | |
Módulo de cizallamiento | 25.9 GPa Show Material materials with Módulo de cizallamiento of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |
Módulo elástico | 69.0 GPa Show Material materials with Módulo elástico of 69.0 GPa | H111 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |
Resistencia a la tracción | 69.0 MPa Show Material materials with Resistencia a la tracción of 69.0 MPa | H111 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 900.0 J/(kg·K) Show Material materials with Calor específico of 900.0 J/(kg·K) | H111 |
Coeficiente de dilatación térmica | 2.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.4e-05 1/K | H111 |
Conductividad térmica | 230.0 W/(m·K) Show Material materials with Conductividad térmica of 230.0 W/(m·K) | H111 |
Temperatura de fusión | 650.0 °C Show Material materials with Temperatura de fusión of 650.0 °C | H111 |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 33000000.0 - 38000000.0 S/m Show Material materials with Conductividad eléctrica of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Resistividad eléctrica | 2.7e-08 - 3e-08 Ω·m Show Material materials with Resistividad eléctrica of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 99.5 - 100.0 % Show Material materials with Aluminio of 99.5 - 100.0 % | H111 |
Boro | 0.05 % Show Material materials with Boro of 0.05 % | H111 |
Cobre | 0.05 % Show Material materials with Cobre of 0.05 % | H111 |
Cromo | 0.01 % Show Material materials with Cromo of 0.01 % | H111 |
Galio | 0.03 % Show Material materials with Galio of 0.03 % | H111 |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | H111 |
Manganeso | 0.01 % Show Material materials with Manganeso of 0.01 % | H111 |
Otro | 0.1 % Show Material materials with Otro of 0.1 % | H111 |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | H111 |
Titanio | 0.02 % Show Material materials with Titanio of 0.02 % | H111 |
Vanadio | 0.02 % Show Material materials with Vanadio of 0.02 % | H111 |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | H111 |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |