General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.7 g/cm³ Show Material materials with Densidad of 8.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 9.2 % Show Material materials with Elongación of 9.2 % |
Límite elástico | 23.0 °C | 1660 MPa Show Material materials with Límite elástico of 1660 MPa |
Módulo elástico | 23.0 °C | 230 GPa Show Material materials with Módulo elástico of 230 GPa |
Resistencia a la tracción | 23.0 °C | 1930 MPa Show Material materials with Resistencia a la tracción of 1930 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K |
Conductividad térmica | 23.0 °C | 11 W/(m·K) Show Material materials with Conductividad térmica of 11 W/(m·K) |
Temperatura de fusión | 1320 °C Show Material materials with Temperatura de fusión of 1320 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.01 % Show Material materials with Azufre of 0 - 0.01 % |
Boro | 0 - 0.015 % Show Material materials with Boro of 0 - 0.015 % |
Carbono | 0 - 0.025 % Show Material materials with Carbono of 0 - 0.025 % |
Cobalto | 29.1 - 39 % Show Material materials with Cobalto of 29.1 - 39 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0 - 0.02 % Show Material materials with Fósforo of 0 - 0.02 % |
Hierro | 0 - 1 % Show Material materials with Hierro of 0 - 1 % |
Manganeso | 0 - 0.15 % Show Material materials with Manganeso of 0 - 0.15 % |
Molibdeno | 9 - 10.5 % Show Material materials with Molibdeno of 9 - 10.5 % |
Níquel | 33 - 37 % Show Material materials with Níquel of 33 - 37 % |
Silicona | 0 - 0.15 % Show Material materials with Silicona of 0 - 0.15 % |
Titanio | 0 - 1 % Show Material materials with Titanio of 0 - 1 % |