General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 17 g/cm³ Show Material materials with Densidad of 17 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Tantalum |
Elongación | 23.0 °C | 1.2 % Show Material materials with Elongación of 1.2 % | |
Límite elástico | 23.0 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa | |
Módulo de cizallamiento | 23.0 °C | 69 GPa Show Material materials with Módulo de cizallamiento of 69 GPa | Typical for Tantalum |
Módulo elástico | 23.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa | |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 140 J/(kg·K) Show Material materials with Calor específico of 140 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 6.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 6.5E-6 1/K | |
Conductividad térmica | 23.0 °C | 52 - 57 W/(m·K) Show Material materials with Conductividad térmica of 52 - 57 W/(m·K) | Typical for Tantalum |
Temperatura de fusión | 2996 °C Show Material materials with Temperatura de fusión of 2996 °C | Typical for Tantalum |
Chemical properties
Property | Value |
---|---|
Carbono | 0 - 0.01 % Show Material materials with Carbono of 0 - 0.01 % |
Hidrógeno | 0 - 1.5E-3 % Show Material materials with Hidrógeno of 0 - 1.5E-3 % |
Hierro | 0 - 0.01 % Show Material materials with Hierro of 0 - 0.01 % |
Molibdeno | 0 - 0.02 % Show Material materials with Molibdeno of 0 - 0.02 % |
Niobio | 0 - 0.1 % Show Material materials with Niobio of 0 - 0.1 % |
Nitrógeno | 0 - 0.01 % Show Material materials with Nitrógeno of 0 - 0.01 % |
Níquel | 0 - 0.01 % Show Material materials with Níquel of 0 - 0.01 % |
Oxígeno | 0 - 0.03 % Show Material materials with Oxígeno of 0 - 0.03 % |
Silicona | 0 - 5E-3 % Show Material materials with Silicona of 0 - 5E-3 % |
Titanio | 0 - 0.01 % Show Material materials with Titanio of 0 - 0.01 % |
Tántalo | 99.7 - 100 % Show Material materials with Tántalo of 99.7 - 100 % |
Wolframio | 0 - 0.05 % Show Material materials with Wolframio of 0 - 0.05 % |