General
Property | Value | Condition |
---|---|---|
Densidad | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ | T6 |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Charpy impact energy, V-notch | 5.0 - 15.0 J Show Material materials with Charpy impact energy, V-notch of 5.0 - 15.0 J | T6 | |||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | T6 | |||
Dureza Brinell | 135 [-] Show Material materials with Dureza Brinell of 135 [-] | T6 | 500 kg load, 10 mm b | ||
Elongación | 4.0 % Show Material materials with Elongación of 4.0 % | T6 | Pink Sheets, ASTM B618 | Casting | A100 |
7.2 % Show Material materials with Elongación of 7.2 % | T6 | ||||
8 % Show Material materials with Elongación of 8 % | T6 | Sand cast, elongation in 50 mm | |||
Límite elástico | 345.0 MPa Show Material materials with Límite elástico of 345.0 MPa | T6 | Pink Sheets, ASTM B618 | Casting | RP02 |
379 MPa Show Material materials with Límite elástico of 379 MPa | T6 | Sand cast, RP02 | |||
400.0 MPa Show Material materials with Límite elástico of 400.0 MPa | T6 | ||||
Módulo de cizallamiento | 23.0 GPa Show Material materials with Módulo de cizallamiento of 23.0 GPa | T6 | |||
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T6 | |||
71 GPa Show Material materials with Módulo elástico of 71 GPa | T6 | ||||
Resistencia a la tracción | 415.0 MPa Show Material materials with Resistencia a la tracción of 415.0 MPa | T6 | Pink Sheets, ASTM B618 | Casting | |
448 MPa Show Material materials with Resistencia a la tracción of 448 MPa | T6 | Sand cast | |||
460.0 MPa Show Material materials with Resistencia a la tracción of 460.0 MPa | T6 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | T6 | ||||
Coeficiente de dilatación térmica | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T6 | ||||
100 °C | 0.0000193 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000193 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
200 °C | 0.0000227 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000227 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
300 °C | 0.0000247 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000247 1/K | T6 | unstated value between 20°C and the mentioned temperature | |||
Conductividad térmica | 120.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 W/(m·K) | T6 | ||||
Temperatura de fusión | 570.0 °C Show Material materials with Temperatura de fusión of 570.0 °C | T6 | ||||
571.0 - 649.0 °C Show Material materials with Temperatura de fusión of 571.0 - 649.0 °C | T6 | Pink Sheets, ASTM B618 | Casting |
Eléctrico
Property | Value | Condition | Comment |
---|---|---|---|
Conductividad eléctrica | 16000000.0 - 19000000.0 S/m Show Material materials with Conductividad eléctrica of 16000000.0 - 19000000.0 S/m | T6 | Typical/Derived values |
Resistividad eléctrica | 5.4e-08 - 6.4e-08 Ω·m Show Material materials with Resistividad eléctrica of 5.4e-08 - 6.4e-08 Ω·m | T6 | Typical values |
Specific Electrical conductivity | 27.0 - 32.0 % IACS Show Material materials with Specific Electrical conductivity of 27.0 - 32.0 % IACS | T6 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 92.1 - 95.1 % Show Material materials with Aluminio of 92.1 - 95.1 % | T6 | ||
Cobre | 4.0 - 5.2 % Show Material materials with Cobre of 4.0 - 5.2 % | T6 | Pink Sheets, ASTM B618 | Casting |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | T6 | ||
0.15 % Show Material materials with Hierro of 0.15 % | T6 | Pink Sheets, ASTM B618 | Casting | |
Magnesio | 0.15 - 0.55 % Show Material materials with Magnesio of 0.15 - 0.55 % | T6 | Pink Sheets, ASTM B618 | Casting |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % | T6 | Pink Sheets, ASTM B618 | Casting |
Otro | 0.1 % Show Material materials with Otro of 0.1 % | T6 | ||
Plata | 0.4 - 1.0 % Show Material materials with Plata of 0.4 - 1.0 % | T6 | Pink Sheets, ASTM B618 | Casting |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | T6 | Pink Sheets, ASTM B618 | Casting |
Titanio | 0.15 - 0.35 % Show Material materials with Titanio of 0.15 - 0.35 % | T6 | Pink Sheets, ASTM B618 | Casting |