General
Property | Value | Condition |
---|---|---|
Densidad | 3.1 g/cm³ Show Material materials with Densidad of 3.1 g/cm³ | T7 |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | T7 | ||||
Dureza Brinell | 130 [-] Show Material materials with Dureza Brinell of 130 [-] | T7 | 500 kg load, 10 mm b | |||
Elongación | 3.0 % Show Material materials with Elongación of 3.0 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting | A100 | |
4.4 % Show Material materials with Elongación of 4.4 % | T7 | |||||
25 °C | 4.5 % Show Material materials with Elongación of 4.5 % | T7 | Sand cast, elongation in 50 mm | |||
105 °C | 7 % Show Material materials with Elongación of 7 % | T7 | Sand cast, elongation in 50 mm | |||
205 °C | 14 % Show Material materials with Elongación of 14 % | T7 | Sand cast, elongation in 50 mm | |||
315 °C | 43 % Show Material materials with Elongación of 43 % | T7 | Sand cast, elongation in 50 mm | |||
Límite elástico | 345.0 MPa Show Material materials with Límite elástico of 345.0 MPa | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting | RP02 | |
410.0 MPa Show Material materials with Límite elástico of 410.0 MPa | T7 | |||||
25 °C | 415 MPa Show Material materials with Límite elástico of 415 MPa | T7 | Sand cast, RP02 | |||
105 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa | T7 | Sand cast, RP02 | |||
205 °C | 150 MPa Show Material materials with Límite elástico of 150 MPa | T7 | Sand cast, RP02 | |||
315 °C | 55 MPa Show Material materials with Límite elástico of 55 MPa | T7 | Sand cast, RP02 | |||
Módulo de cizallamiento | 23.0 GPa Show Material materials with Módulo de cizallamiento of 23.0 GPa | T7 | ||||
Módulo elástico | 71.0 GPa Show Material materials with Módulo elástico of 71.0 GPa | T7 | ||||
71 GPa Show Material materials with Módulo elástico of 71 GPa | T7 | |||||
Resistencia a la fluencia | 150 °C | 270 MPa Show Material materials with Resistencia a la fluencia of 270 MPa | T7 | up to 1000 hours | ||
175 °C | 180 MPa Show Material materials with Resistencia a la fluencia of 180 MPa | T7 | up to 1000 hours | |||
205 °C | 130 MPa Show Material materials with Resistencia a la fluencia of 130 MPa | T7 | up to 1000 hours | |||
230 °C | 95 MPa Show Material materials with Resistencia a la fluencia of 95 MPa | T7 | up to 1000 hours | |||
260 °C | 70 MPa Show Material materials with Resistencia a la fluencia of 70 MPa | T7 | up to 1000 hours | |||
290 °C | 48 MPa Show Material materials with Resistencia a la fluencia of 48 MPa | T7 | up to 1000 hours | |||
315 °C | 31 MPa Show Material materials with Resistencia a la fluencia of 31 MPa | T7 | up to 1000 hours | |||
Resistencia a la tracción | 415.0 MPa Show Material materials with Resistencia a la tracción of 415.0 MPa | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting | ||
470.0 MPa Show Material materials with Resistencia a la tracción of 470.0 MPa | T7 | |||||
25 °C | 467 MPa Show Material materials with Resistencia a la tracción of 467 MPa | T7 | Sand cast | |||
105 °C | 315 MPa Show Material materials with Resistencia a la tracción of 315 MPa | T7 | Sand cast | |||
205 °C | 185 MPa Show Material materials with Resistencia a la tracción of 185 MPa | T7 | Sand cast | |||
315 °C | 60 MPa Show Material materials with Resistencia a la tracción of 60 MPa | T7 | Sand cast |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | 920.0 J/(kg·K) Show Material materials with Calor específico of 920.0 J/(kg·K) | T7 | ||||
Coeficiente de dilatación térmica | 2.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1e-05 1/K | T7 | ||||
100 °C | 0.0000193 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000193 1/K | T7 | unstated value between 20°C and the mentioned temperature | |||
200 °C | 0.0000227 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000227 1/K | T7 | unstated value between 20°C and the mentioned temperature | |||
300 °C | 0.0000247 1/K Show Material materials with Coeficiente de dilatación térmica of 0.0000247 1/K | T7 | unstated value between 20°C and the mentioned temperature | |||
Conductividad térmica | 120.0 W/(m·K) Show Material materials with Conductividad térmica of 120.0 W/(m·K) | T7 | ||||
Temperatura de fusión | 570.0 °C Show Material materials with Temperatura de fusión of 570.0 °C | T7 | ||||
571.0 - 649.0 °C Show Material materials with Temperatura de fusión of 571.0 - 649.0 °C | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Eléctrico
Property | Value | Condition | Comment |
---|---|---|---|
Conductividad eléctrica | 19000000 S/m Show Material materials with Conductividad eléctrica of 19000000 S/m | T7 | Typical/Derived values |
Resistividad eléctrica | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Resistividad eléctrica of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium | |
Specific Electrical conductivity | 32.0 - 34.0 % IACS Show Material materials with Specific Electrical conductivity of 32.0 - 34.0 % IACS | T7 | Typical values |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 92.1 - 95.1 % Show Material materials with Aluminio of 92.1 - 95.1 % | T7 | ||
Cobre | 4.0 - 5.2 % Show Material materials with Cobre of 4.0 - 5.2 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | T7 | ||
0.15 % Show Material materials with Hierro of 0.15 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting | |
Magnesio | 0.15 - 0.55 % Show Material materials with Magnesio of 0.15 - 0.55 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Otro | 0.1 % Show Material materials with Otro of 0.1 % | T7 | ||
Plata | 0.4 - 1.0 % Show Material materials with Plata of 0.4 - 1.0 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |
Titanio | 0.15 - 0.35 % Show Material materials with Titanio of 0.15 - 0.35 % | T7 | Pink Sheets, ASTM B26, ASTM B618 | Casting |