General
Property | Value | Condition |
---|---|---|
Densidad | 3.0 g/cm³ Show Material materials with Densidad of 3.0 g/cm³ | T3510 |
Mecánica
Property | Value | Condition | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |
Elongación | 6.9 % Show Material materials with Elongación of 6.9 % | T3510 | |
Límite elástico | 330.0 MPa Show Material materials with Límite elástico of 330.0 MPa | T3510 | |
Módulo de cizallamiento | 26.0 - 27.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 27.5 GPa | Typical for Wrought 2000 Series Aluminium | |
Módulo elástico | 73.0 GPa Show Material materials with Módulo elástico of 73.0 GPa | T3510 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |
Resistencia a la tracción | 440.0 MPa Show Material materials with Resistencia a la tracción of 440.0 MPa | T3510 |
Aplicaciones térmicas
Property | Value | Condition |
---|---|---|
Calor específico | 870.0 J/(kg·K) Show Material materials with Calor específico of 870.0 J/(kg·K) | T3510 |
Coeficiente de dilatación térmica | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T3510 |
Conductividad térmica | 150.0 W/(m·K) Show Material materials with Conductividad térmica of 150.0 W/(m·K) | T3510 |
Temperatura de fusión | 510.0 °C Show Material materials with Temperatura de fusión of 510.0 °C | T3510 |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 18000000.0 - 30000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 30000000.0 S/m | Typical for Wrought 2000 Series Aluminium |
Resistividad eléctrica | 3.4e-08 - 6e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.4e-08 - 6e-08 Ω·m | Typical for Wrought 2000 Series Aluminium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 90.4 - 95.0 % Show Material materials with Aluminio of 90.4 - 95.0 % | T3510 |
Circonio | 0.2 % Show Material materials with Circonio of 0.2 % | T3510 |
Cobre | 3.9 - 5.0 % Show Material materials with Cobre of 3.9 - 5.0 % | T3510 |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T3510 |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | T3510 |
Magnesio | 0.2 - 0.8 % Show Material materials with Magnesio of 0.2 - 0.8 % | T3510 |
Manganeso | 0.4 - 1.2 % Show Material materials with Manganeso of 0.4 - 1.2 % | T3510 |
Otro | 0.15 % Show Material materials with Otro of 0.15 % | T3510 |
Silicona | 0.5 - 1.2 % Show Material materials with Silicona of 0.5 - 1.2 % | T3510 |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | T3510 |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T3510 |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |