General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9 g/cm³ Show Material materials with Densidad of 9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Límite elástico | 23.0 °C | 320 MPa Show Material materials with Límite elástico of 320 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa | |
Resistencia a la tracción | 23.0 °C | 360 MPa Show Material materials with Resistencia a la tracción of 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 390 J/(kg·K) Show Material materials with Calor específico of 390 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 23.0 °C | 390 W/(m·K) Show Material materials with Conductividad térmica of 390 W/(m·K) |
Temperatura de fusión | 1080 °C Show Material materials with Temperatura de fusión of 1080 °C |
Chemical properties
Property | Value |
---|---|
Cobre | 99.9 - 100 % Show Material materials with Cobre of 99.9 - 100 % |
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |