General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.2 g/cm³ Show Supplier Material materials with Densidad of 4.2 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 390 GPa Show Supplier Material materials with Módulo elástico of 390 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 7 - 9 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 7 - 9 MPa·√m |
Resistencia a la flexión | 23.0 °C | 700 MPa Show Supplier Material materials with Resistencia a la flexión of 700 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 35 W/(m·K) Show Supplier Material materials with Conductividad térmica of 35 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.15E-5 Ω·m Show Supplier Material materials with Resistividad eléctrica of 3.15E-5 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: Cutting tool inserts, stamping tool parts, wear resistant parts |