General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 5.4 g/cm³ Show Supplier Material materials with Densidad of 5.4 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 1130 [-] Show Supplier Material materials with Dureza Vickers of 1130 [-] | |
Módulo elástico | 23.0 °C | 260 GPa Show Supplier Material materials with Módulo elástico of 260 GPa | |
Módulos de Weibull | 23.0 °C | 16.8 [-] Show Supplier Material materials with Módulos de Weibull of 16.8 [-] | |
Plane-Strain Fracture Toughnes | 23.0 °C | 10 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 10 MPa·√m | SENVB |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9.3E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.3E-6 1/K |
Conductividad térmica | 23.0 °C | 10 W/(m·K) Show Supplier Material materials with Conductividad térmica of 10 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: Structural applications with high loading conditions | |
Other | The synthesis and processing of this composition is a patented procedure (patent no WO2011/015697 A1) |