General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 3.94 g/cm³ Show Supplier Material materials with Densidad of 3.94 g/cm³ | |
Porosidad | 0 % Show Supplier Material materials with Porosidad of 0 % | open porositiy |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 380 GPa Show Supplier Material materials with Módulo elástico of 380 GPa |
Plane-Strain Fracture Toughnes | 23.0 °C | 3.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 3.8 MPa·√m |
Resistencia a la flexión | 23.0 °C | 420 MPa Show Supplier Material materials with Resistencia a la flexión of 420 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 1000.0 °C | 8.5E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.5E-6 1/K | |
Conductividad térmica | 23.0 °C | 29 W/(m·K) Show Supplier Material materials with Conductividad térmica of 29 W/(m·K) | |
Temperatura máx. de funcionamiento | 1750 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1750 °C | no load |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+11 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+11 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.96 % Show Supplier Material materials with Aluminio of 99.96 % | as Al₂O₃ |
Calcio | 1E-3 % Show Supplier Material materials with Calcio of 1E-3 % | as CaO |
Cromo | 1E-3 % Show Supplier Material materials with Cromo of 1E-3 % | |
Hierro | 0.01 % Show Supplier Material materials with Hierro of 0.01 % | as Fe₂O₃ |
Magnesio | 3E-3 % Show Supplier Material materials with Magnesio of 3E-3 % | as MgO |
Silicona | 0.01 % Show Supplier Material materials with Silicona of 0.01 % | as SiO₂ |
Titanio | 3E-3 % Show Supplier Material materials with Titanio of 3E-3 % | as TiO₂ |
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: High temperature labware, furnace construction, abrasives industry, pump & compressor industry, chemical & pharma industry |