General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 5.5 g/cm³ Show Supplier Material materials with Densidad of 5.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 1400 [-] Show Supplier Material materials with Dureza Vickers of 1400 [-] | |
Módulo elástico | 23.0 °C | 275 GPa Show Supplier Material materials with Módulo elástico of 275 GPa | |
Plane-Strain Fracture Toughnes | 23.0 °C | 5 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 5 MPa·√m | |
Resistencia a la flexión | 23.0 °C | 1550 MPa Show Supplier Material materials with Resistencia a la flexión of 1550 MPa | after HIP |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 1000.0 °C | 1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | |
Conductividad térmica | 23.0 °C | 5.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 5.6 W/(m·K) | |
Temperatura máx. de funcionamiento | 1450 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1450 °C | no load |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+11 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.00E+11 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 20 % Show Supplier Material materials with Aluminio of 20 % | as Al₂O₃ |
Circonio | 76 % Show Supplier Material materials with Circonio of 76 % | as ZrO₂ |
Itrio | 3.9 % Show Supplier Material materials with Itrio of 3.9 % | as Y₂O₃ |
Silicona | 0.02 % Show Supplier Material materials with Silicona of 0.02 % | as SiO₂ |
Sodio | 0.04 % Show Supplier Material materials with Sodio of 0.04 % | as Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | Typical application areas include: Pump & compressor industry, seal & gasket industry, wear parts, grinding media, bio applications (implants) |