General
Property | Value |
---|---|
Densidad | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Strip thickness 0.08 - 3.0 mm, other gauges on request. Strip width from 8.5 mm. Hot-dip tinned and electroplated strip available. |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.33 [-] | ||
Dureza Vickers | 145 - 175 [-] Show Supplier Material materials with Dureza Vickers of 145 - 175 [-] | R490(TM04) | For reference only | |
150 - 180 [-] Show Supplier Material materials with Dureza Vickers of 150 - 180 [-] | R520(TM06) | For reference only | ||
180 - 220 [-] Show Supplier Material materials with Dureza Vickers of 180 - 220 [-] | R580(TM08) | For reference only | ||
Elongación | 6 % Show Supplier Material materials with Elongación of 6 % | min. | R580(TM08), A50 | |
8 % Show Supplier Material materials with Elongación of 8 % | min. | R520(TM06), A50 | ||
10 % Show Supplier Material materials with Elongación of 10 % | min. | R490(TM04), A50 | ||
Límite elástico | 410 MPa Show Supplier Material materials with Límite elástico of 410 MPa | min. | R490(TM04) | |
460 MPa Show Supplier Material materials with Límite elástico of 460 MPa | min. | R520(TM06) | ||
520 MPa Show Supplier Material materials with Límite elástico of 520 MPa | min. | R580(TM08) | ||
Módulo elástico | 130 GPa Show Supplier Material materials with Módulo elástico of 130 GPa | ||
Plegabilidad 180 ° bidireccional | 2 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 2 [-] | ASTM B820 | R490(TM04) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
2 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 2 [-] | ASTM B820 | R520(TM06) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
3 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 3 [-] | ASTM B820 | R580(TM08) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 180 ° en peso bruto | 1.5 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 1.5 [-] | ASTM B820 | R490(TM04) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
1.5 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 1.5 [-] | ASTM B820 | R520(TM06) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 2 [-] | ASTM B820 | R580(TM08) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° bidireccional | 1 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 [-] | EN ISO 7438 | R490(TM04) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 [-] | EN ISO 7438 | R580(TM08) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | EN ISO 7438 | R520(TM06) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° en peso bruto | 0.8 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0.8 [-] | EN ISO 7438 | R490(TM04) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | EN ISO 7438 | R520(TM06) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | EN ISO 7438 | R580(TM08) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Resistencia a la tracción | 490 - 560 MPa Show Supplier Material materials with Resistencia a la tracción of 490 - 560 MPa | R490(TM04) | |
520 - 590 MPa Show Supplier Material materials with Resistencia a la tracción of 520 - 590 MPa | R520(TM06) | ||
580 - 655 MPa Show Supplier Material materials with Resistencia a la tracción of 580 - 655 MPa | R580(TM08) |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 377 J/(kg·K) Show Supplier Material materials with Calor específico of 377 J/(kg·K) | ||
Coeficiente de dilatación térmica | 1.68e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.68e-05 1/K | average value between 20-300°C | |
Conductividad térmica | 20 °C | 260 W/(m·K) Show Supplier Material materials with Conductividad térmica of 260 W/(m·K) |
Eléctrico
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Application target: Ideal for power connectors. | |
Chemical composition | The chemical composition is the nominal composition of the alloy | |
Coating | Electroplating: Good Hot dip tinning: Good | |
Cold Forming | Good | |
Machining | Fair | |
Packaging size | Standard coils with outside diameters up to 1200 mm. Traverse-wound coils with drum weights up to 500 kg. Multiple-coil up to 3 tons. | |
Soldering general | Soft soldering: Good | |
Testings | Fatigue strength: The fatigue strength is defined as the maximum bending stress amplitude which a material withstands for 10.000.000 load cycles under symmetrical alternate load without breaking. It depends on the temper selected and can be estimated typically by 1/3 of tensile strength. For solid solution fine grain materials fatigue strength might increase up to 0,5 * of tensile strength. Bending test: 90° bend test According to EN ISO 7438, 180° bend test acc. to ASTM B820, shown values might show orange- peel, however no crack. | |
Welding | Laser welding: Suitable Resistance welding: Average |