Acero bajo en carbono
EN 10149-2 Grade S460MC thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-3 Grade S460N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-3 Grade S460NL normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML1 thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-6 Grade S460QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10225 Grade S460G1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P460QH quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460M thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch