General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.83 g/cm³ Show Supplier Material materials with Densidad of 7.83 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1350 - 2540 mm Show Supplier Material materials with Ancho of 1350 - 2540 mm |
Diámetro exterior | 450 - 910 mm Show Supplier Material materials with Diámetro exterior of 450 - 910 mm |
Diámetro interior | 400 - 730 mm Show Supplier Material materials with Diámetro interior of 400 - 730 mm |
Espesor | 150 - 230 mm Show Supplier Material materials with Espesor of 150 - 230 mm |
Longitud | 1750 - 3370 mm Show Supplier Material materials with Longitud of 1750 - 3370 mm |
Chemical properties
Property | Value |
---|---|
Arsénico | 0 - 0.08 % Show Supplier Material materials with Arsénico of 0 - 0.08 % |
Azufre | 0 - 0.04 % Show Supplier Material materials with Azufre of 0 - 0.04 % |
Carbono | 0.42 - 0.5 % Show Supplier Material materials with Carbono of 0.42 - 0.5 % |
Cobre | 0 - 0.25 % Show Supplier Material materials with Cobre of 0 - 0.25 % |
Cromo | 0 - 0.25 % Show Supplier Material materials with Cromo of 0 - 0.25 % |
Fósforo | 0 - 0.04 % Show Supplier Material materials with Fósforo of 0 - 0.04 % |
Hierro | Balance |
Manganeso | 0.5 - 0.8 % Show Supplier Material materials with Manganeso of 0.5 - 0.8 % |
Níquel | 0 - 0.25 % Show Supplier Material materials with Níquel of 0 - 0.25 % |
Silicona | 0.17 - 0.37 % Show Supplier Material materials with Silicona of 0.17 - 0.37 % |
Technological properties
Property | ||
---|---|---|
Application areas | Steel forgings are applied for manufacture of the details of machinery and spare parts for metallurgical, mining and machine-building equipment. | |
Processing methods | Manufactured by open die forging |