Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 1400 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1400 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Circonio | 0.06 - 0.12 % Show Supplier Material materials with Circonio of 0.06 - 0.12 % |
Cobre | 2E-4 % Show Supplier Material materials with Cobre of 2E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 5E-4 % Show Supplier Material materials with Hierro of 5E-4 % |
Molibdeno | balance |
Nitrógeno | 5E-4 % Show Supplier Material materials with Nitrógeno of 5E-4 % |
Níquel | 1E-4 % Show Supplier Material materials with Níquel of 1E-4 % |
Oxígeno | 0.01 % Show Supplier Material materials with Oxígeno of 0.01 % |
Potasio | 6E-4 % Show Supplier Material materials with Potasio of 6E-4 % |
Silicona | 2E-4 % Show Supplier Material materials with Silicona of 2E-4 % |
Titanio | 0.4 - 0.55 % Show Supplier Material materials with Titanio of 0.4 - 0.55 % |
Wolframio | 0.02 % Show Supplier Material materials with Wolframio of 0.02 % |
Technological properties
Property | ||
---|---|---|
Application areas | TZM is used in high-temperature applications involving demanding mechanical loads, for example in forging tools or as rotating anodes in X-ray tubes. The recommended temperatures of use are between 700 and 1400 °C. |