General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.15 g/cm³ Show Supplier Material materials with Densidad of 7.15 g/cm³ |
Masa molar | 52 g/mol Show Supplier Material materials with Masa molar of 52 g/mol |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.21 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.21 [-] |
Dureza Vickers 10 | 23.0 °C | 180 - 250 [-] Show Supplier Material materials with Dureza Vickers 10 of 180 - 250 [-] |
Módulo elástico | 23.0 °C | 290 GPa Show Supplier Material materials with Módulo elástico of 290 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Supplier Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 6.2E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.2E-6 1/K |
Conductividad térmica | 23.0 °C | 93.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 93.7 W/(m·K) |
Punto de ebullición | 2672 °C Show Supplier Material materials with Punto de ebullición of 2672 °C | |
Temperatura de fusión | 1900 °C Show Supplier Material materials with Temperatura de fusión of 1900 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 7.90E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 7.90E+6 S/m |
Función de trabajo | 23.0 °C | 4.5 eV Show Supplier Material materials with Función de trabajo of 4.5 eV |
Resistividad eléctrica | 23.0 °C | 1.3E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 1.3E-7 Ω·m |
Acústico
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | ||
Cromo | 99.8 % Show Supplier Material materials with Cromo of 99.8 % | min | |
Hierro | 0.15 % Show Supplier Material materials with Hierro of 0.15 % | ||
Molibdeno | 0.005 | ||
Nitrógeno | 0.02 % Show Supplier Material materials with Nitrógeno of 0.02 % | ||
Otro | 0.03 % Show Supplier Material materials with Otro of 0.03 % | ||
Oxígeno | 0.1 % Show Supplier Material materials with Oxígeno of 0.1 % | ||
Silicona | 0.05 % Show Supplier Material materials with Silicona of 0.05 % | ||
Wolframio | 5E-3 % Show Supplier Material materials with Wolframio of 5E-3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thanks to its very high corrosion resistance against many different acids and bases as well as hot gases, chromium is a popular material for all types of protective coating. In combustion equipment, chromium is used as a wear-resistant coating to increase the service life of specific components. As a component in high-temperature fuel cells, chromium also performs brilliantly. Alongside these applications, chromium is also used as a brilliant decorative coating for operating elements on appliances or for jewellery. |