General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 19.3 g/cm³ Show Supplier Material materials with Densidad of 19.3 g/cm³ |
Masa molar | 183.85 g/mol Show Supplier Material materials with Masa molar of 183.85 g/mol |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.28 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.28 [-] | |
Dureza Vickers 30 | 23.0 °C | 360 [-] Show Supplier Material materials with Dureza Vickers 30 of 360 [-] | recrystallized |
Módulo elástico | 23.0 °C | 405 GPa Show Supplier Material materials with Módulo elástico of 405 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 130 J/(kg·K) Show Supplier Material materials with Calor específico of 130 J/(kg·K) |
Conductividad térmica | 23.0 °C | 164 W/(m·K) Show Supplier Material materials with Conductividad térmica of 164 W/(m·K) |
Temperatura de fusión | 3420 °C Show Supplier Material materials with Temperatura de fusión of 3420 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.80E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.80E+7 S/m |
Función de trabajo | 23.0 °C | 4.54 eV Show Supplier Material materials with Función de trabajo of 4.54 eV |
Resistividad eléctrica | 23.0 °C | 5E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5E-8 Ω·m |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 6E-4 % Show Supplier Material materials with Carbono of 6E-4 % |
Cobre | 1E-4 % Show Supplier Material materials with Cobre of 1E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 8E-4 % Show Supplier Material materials with Hierro of 8E-4 % |
Molibdeno | 1.2E-3 % Show Supplier Material materials with Molibdeno of 1.2E-3 % |
Nitrógeno | 1E-4 % Show Supplier Material materials with Nitrógeno of 1E-4 % |
Níquel | 2E-4 % Show Supplier Material materials with Níquel of 2E-4 % |
Oxígeno | 2E-4 % Show Supplier Material materials with Oxígeno of 2E-4 % |
Plomo | 1E-4 % Show Supplier Material materials with Plomo of 1E-4 % |
Potasio | 1E-4 % Show Supplier Material materials with Potasio of 1E-4 % |
Silicona | 1E-4 % Show Supplier Material materials with Silicona of 1E-4 % |
Wolframio | 99.97 % Show Supplier Material materials with Wolframio of 99.97 % |
Technological properties
Property | ||
---|---|---|
Application areas | For example, this material can be used to manufacture high-temperature furnace components, lamp components and components for use in the fields of medical and thin-film technology. |