General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 19.3 g/cm³ Show Supplier Material materials with Densidad of 19.3 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 0.64 - 1 mm Show Supplier Material materials with Diámetro of 0.64 - 1 mm |
Dimensions | Available diameters (mm): 0.635; 0.76; 1 |
Chemical properties
Property | Value |
---|---|
Aluminio | 3E-3 % Show Supplier Material materials with Aluminio of 3E-3 % |
Cadmio | 5E-4 % Show Supplier Material materials with Cadmio of 5E-4 % |
Carbono | 3E-3 % Show Supplier Material materials with Carbono of 3E-3 % |
Cobre | 1E-3 % Show Supplier Material materials with Cobre of 1E-3 % |
Cromo | 2E-3 % Show Supplier Material materials with Cromo of 2E-3 % |
Hierro | 3E-3 % Show Supplier Material materials with Hierro of 3E-3 % |
Mercurio | 1E-4 % Show Supplier Material materials with Mercurio of 1E-4 % |
Molibdeno | 0.01 % Show Supplier Material materials with Molibdeno of 0.01 % |
Nitrógeno | 1E-3 % Show Supplier Material materials with Nitrógeno of 1E-3 % |
Níquel | 2E-3 % Show Supplier Material materials with Níquel of 2E-3 % |
Oxígeno | 5E-3 % Show Supplier Material materials with Oxígeno of 5E-3 % |
Plomo | 5E-4 % Show Supplier Material materials with Plomo of 5E-4 % |
Potasio | 3E-3 - 7E-3 % Show Supplier Material materials with Potasio of 3E-3 - 7E-3 % |
Silicona | 3E-3 % Show Supplier Material materials with Silicona of 3E-3 % |
Wolframio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | WVM is primarily supplied in rod or wire form for use in evaporation coils or heating filaments. |