General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 17.15 - 17.85 g/cm³ Show Supplier Material materials with Densidad of 17.15 - 17.85 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 6 mm Show Supplier Material materials with Diámetro of 6 mm |
Longitud | 330 mm Show Supplier Material materials with Longitud of 330 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 6 x 330; 8 x 330; 10 x 330; 12 x 330; 14 x 320; 16 x 320; 18 x 320; 20 x 500; 22 x 500; 24 x 500; 26 x 500; 28 x 500; 30 x 500; 32 x 500; 37 x 500; 42 x 600; 47 x 600; 52 x 600; 57 x 700; 62 x 700 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 270 - 330 [-] Show Supplier Material materials with Dureza Vickers 10 of 270 - 330 [-] |
Límite elástico Rp 0,2 | 23.0 °C | 517 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 517 MPa |
Módulo elástico | 23.0 °C | 360 GPa Show Supplier Material materials with Módulo elástico of 360 GPa |
Chemical properties
Property | Value |
---|---|
Hierro | 2 - 3 % Show Supplier Material materials with Hierro of 2 - 3 % |
Níquel | 4.5 - 5.5 % Show Supplier Material materials with Níquel of 4.5 - 5.5 % |
Wolframio | 91.5 - 93.5 % Show Supplier Material materials with Wolframio of 91.5 - 93.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Weakly ferromagnetic, DENSIMET® D176 is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006. |