General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 18.25 - 18.85 g/cm³ Show Supplier Material materials with Densidad of 18.25 - 18.85 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 30 - 70 mm Show Supplier Material materials with Diámetro of 30 - 70 mm |
Longitud | 250 - 500 mm Show Supplier Material materials with Longitud of 250 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 30 x 500; 40 x 500; 70 x 250 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 23.0 °C | 270 - 330 [-] Show Supplier Material materials with Dureza Vickers 10 of 270 - 330 [-] |
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % |
Límite elástico Rp 0,2 | 23.0 °C | 517 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 517 MPa |
Resistencia a la tracción | 23.0 °C | 689 MPa Show Supplier Material materials with Resistencia a la tracción of 689 MPa |
Chemical properties
Property | Value |
---|---|
Hierro | 0.5 - 1.5 % Show Supplier Material materials with Hierro of 0.5 - 1.5 % |
Níquel | 1.5 - 2.5 % Show Supplier Material materials with Níquel of 1.5 - 2.5 % |
Wolframio | 96 - 98 % Show Supplier Material materials with Wolframio of 96 - 98 % |
Technological properties
Property | ||
---|---|---|
Application areas | Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Weakly ferromagnetic, DENSIMET® D185ND is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006. |