General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 16.9 - 17.6 g/cm³ Show Supplier Material materials with Densidad of 16.9 - 17.6 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 10 - 40 mm Show Supplier Material materials with Diámetro of 10 - 40 mm |
Longitud | 250 - 500 mm Show Supplier Material materials with Longitud of 250 - 500 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 10 x 250; 12 x 250; 16 x 250; 20 x 500; 25 x 500; 30 x 500; 40 x 500 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 23.0 °C | 31 [-] Show Supplier Material materials with Dureza Rockwell C of 31 [-] |
Dureza Vickers 10 | 23.0 °C | 300 - 360 [-] Show Supplier Material materials with Dureza Vickers 10 of 300 - 360 [-] |
Elongación | 23.0 °C | 4 - 18 % Show Supplier Material materials with Elongación of 4 - 18 % |
Límite elástico | 23.0 °C | 700 MPa Show Supplier Material materials with Límite elástico of 700 MPa |
Límite elástico Rp 0,2 | 23.0 °C | 550 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 550 MPa |
Módulo elástico | 23.0 °C | 360 GPa Show Supplier Material materials with Módulo elástico of 360 GPa |
Resistencia a la tracción | 23.0 °C | 800 - 990 MPa Show Supplier Material materials with Resistencia a la tracción of 800 - 990 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.3E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.3E-6 1/K |
Conductividad térmica | 500.0 °C | 65 W/(m·K) Show Supplier Material materials with Conductividad térmica of 65 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Hierro | 1.5 - 2.5 % Show Supplier Material materials with Hierro of 1.5 - 2.5 % |
Molibdeno | 3.5 - 4.5 % Show Supplier Material materials with Molibdeno of 3.5 - 4.5 % |
Níquel | 3.5 - 4.5 % Show Supplier Material materials with Níquel of 3.5 - 4.5 % |
Wolframio | 88.5 - 91.5 % Show Supplier Material materials with Wolframio of 88.5 - 91.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Densimet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Weakly ferromagnetic, DENSIMET® D2M is according to RoHS directives (EU2002/95/EG, EU2000/53/EG, EU2006/122/EG) and REACH Regulation EC 1907/2006. |