General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 17.6 g/cm³ Show Supplier Material materials with Densidad of 17.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 350 GPa Show Supplier Material materials with Módulo elástico of 350 GPa |
Chemical properties
Property | Value |
---|---|
Cobre | binder |
Níquel | binder |
Wolframio | 92.5 % Show Supplier Material materials with Wolframio of 92.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Inermet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Paramagnetic |